Tue, 19 Feb 2002 15:24:35 +0800
MIME-Version:
1.0
X-To:
Don Vischulis <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (110 lines)
Calvin,

My further 2 cents worth is that since MIL-STD-2118 Notice 2 states that
the spec is cancelled and refers you to IPC-2223 or IPC-2221 instead, this
should be sufficient authorisation to use the IPC spec instead. i.e.

* Drg calls up MIL-STD-2118.
* You look up the MIL std and it tells you it's superseded another spec
(IPC-2223)
* You can then legitimately look up IPC-2223 as if it were MIL-STD-2118 and
read it as the requirement called up in the old drawings.

I can't vouch for whether or not there is any difference between the MIL
std content and the IPC std content, insofar as they cross-relate, but
there is no logical or arguable reason why you shouldn't be simplistic and
use the IPC std as if it were the MIL std called up in your drawings.

Peter




                    Don Vischulis
                    <dvischulis@W        To:     [log in to unmask]
                    I.RR.COM>            cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     Re: [TN] MIL-P-50884 and MIL-STD-2118
                    <[log in to unmask]
                    ORG>


                    02/19/02
                    06:59 AM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum.";
                    Please
                    respond to
                    Don Vischulis






Calvin,

Go to the DSCC web site
http://www.dscc.dla.mil/Programs/MilSpec/DocSearch.asp and enter the
numeric for your specs in the search box.  I didn't check both, but 50884
is available as a pdf file.

Don Vischulis

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Calvin Reynard
Sent: Monday, February 18, 2002 3:41 PM
To: [log in to unmask]
Subject: [TN] MIL-P-50884 and MIL-STD-2118

Hello, everyone,

I am looking for MIL-P-50884 and MIL-STD-2118 (Flex, Rigid-Flex specs) that
are not longer active.
I know IPC-2223 replaces them but everybody list these specs in their
documentation. Can anyone help?

I found several sites that list them but the links are dead.

Thanks,

              \\\|///
              ( 0 0 )
+---------oOOO--(_)--OOOo---------+
|                                 |
| Calvin Reynard                  |
| Securaplane Technologies        |
| 10800 N. Mavinee Dr.            |
| Tucson, AZ 85737                |
|                                 |
| Voice   520-297-0844            |
| Fax     520-498-49241           |
| Email   [log in to unmask]  |
|                                 |
|         ooooO                   |
|         (   )   Ooooo           |
+----------\ (----(   )-----------+
            \_)    ) /
                  (_/



[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2