Calvin, My further 2 cents worth is that since MIL-STD-2118 Notice 2 states that the spec is cancelled and refers you to IPC-2223 or IPC-2221 instead, this should be sufficient authorisation to use the IPC spec instead. i.e. * Drg calls up MIL-STD-2118. * You look up the MIL std and it tells you it's superseded another spec (IPC-2223) * You can then legitimately look up IPC-2223 as if it were MIL-STD-2118 and read it as the requirement called up in the old drawings. I can't vouch for whether or not there is any difference between the MIL std content and the IPC std content, insofar as they cross-relate, but there is no logical or arguable reason why you shouldn't be simplistic and use the IPC std as if it were the MIL std called up in your drawings. Peter Don Vischulis <dvischulis@W To: [log in to unmask] I.RR.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Sent by: Aero/ST Group) TechNet Subject: Re: [TN] MIL-P-50884 and MIL-STD-2118 <[log in to unmask] ORG> 02/19/02 06:59 AM Please respond to "TechNet E-Mail Forum."; Please respond to Don Vischulis Calvin, Go to the DSCC web site http://www.dscc.dla.mil/Programs/MilSpec/DocSearch.asp and enter the numeric for your specs in the search box. I didn't check both, but 50884 is available as a pdf file. Don Vischulis -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Calvin Reynard Sent: Monday, February 18, 2002 3:41 PM To: [log in to unmask] Subject: [TN] MIL-P-50884 and MIL-STD-2118 Hello, everyone, I am looking for MIL-P-50884 and MIL-STD-2118 (Flex, Rigid-Flex specs) that are not longer active. I know IPC-2223 replaces them but everybody list these specs in their documentation. Can anyone help? I found several sites that list them but the links are dead. Thanks, \\\|/// ( 0 0 ) +---------oOOO--(_)--OOOo---------+ | | | Calvin Reynard | | Securaplane Technologies | | 10800 N. Mavinee Dr. | | Tucson, AZ 85737 | | | | Voice 520-297-0844 | | Fax 520-498-49241 | | Email [log in to unmask] | | | | ooooO | | ( ) Ooooo | +----------\ (----( )-----------+ \_) ) / (_/ [This e-mail is confidential and may also be privileged. If you are not the intended recipient, please delete it and notify us immediately; you should not copy or use it for any purpose, nor disclose its contents to any other person. Thank you.] --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8d To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------