TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 24 Aug 1999 01:23:00 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
Jon Moore <[log in to unmask]>
Parts/Attachments:
text/plain (42 lines)
In a message dated 8/20/99 11:51:49 AM US Eastern Standard Time,
[log in to unmask] writes:

<< We are about to start using BGAs in our designs.  Can anyone recommend a
BGA
 rework station and BGA inspection equipment to inspect for poor alignment,
 solder cracks,poor soldering, etc.  Is there X-ray equipment that will
highlight
 defects by enhancing the image with a different color to call out a possible
 defect?  What features should we look for in both kinds of equipment?  The
PCA's
 are manufactured off site and sent to my facility for testing and
incorporation
 into the product.  Any help would be appreciated.  Thank you in advance.

 Best Regards,

 Mike Forrester
 LeCroy Corp >>
Mike,
    I would recommend Pace Thermo-Flo for your BGA rework needs.  As for
X-ray equipment, LIXI makes an excellent table-top system that uses a Mantis
viewer for looking at the solder connections in real time x-ray.  The
resolution will not reveal minor cracks, etc., but it is a very good
production process evaluation tool for alignment, bridging, etc.

Jon Moore

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2