TECHNET Archives

January 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Richard Kraszewski <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Thu, 22 Jan 2004 16:33:06 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Yes . More than likely organics acids & resins. 

Rich Kraszewski 
Advanced Manufacturing Engineer - KEDS
Phone:  260.925.8919
Pager:  812.481.3492
 
 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Park
Sent: Thursday, January 22, 2004 4:18 PM
To: [log in to unmask]
Subject: [TN] white no clean flux residue


I'm seeking input/confirmation about a problem I am observing for no
clean wave soldering process. The problem is a constant build-up of
white powdery flux residue in/around flux spray system. Our wave
operators remove the residue around spray nozzle every 2/4 hours with
brush/alcohol. It gets build-up quickly around the whole spray flux
system.

Boards that are wave processed have invisible white residue. It requires
a clean wipe to see some. This flux is alcohol-based no clean with 2%
resin as solid content. I am used to using alcohol-based no clean with
organic chemistry as flux activator and didn't have any issue with white
flux residue build-up.

J-STD-004 calls out four classifications of flux composition
(Rosin/Resin/Organic/Inorganic). Is white powdery residue build-up from
resin formulation in the flux we are using?

any thoughts?
thanks


Matthew S. Park
Preco Electronics
tel: (309)-263-7788
fax: (309)-266-6674
1651 N. Main Morton. IL 61550

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2