Yes . More than likely organics acids & resins. Rich Kraszewski Advanced Manufacturing Engineer - KEDS Phone: 260.925.8919 Pager: 812.481.3492 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Matthew Park Sent: Thursday, January 22, 2004 4:18 PM To: [log in to unmask] Subject: [TN] white no clean flux residue I'm seeking input/confirmation about a problem I am observing for no clean wave soldering process. The problem is a constant build-up of white powdery flux residue in/around flux spray system. Our wave operators remove the residue around spray nozzle every 2/4 hours with brush/alcohol. It gets build-up quickly around the whole spray flux system. Boards that are wave processed have invisible white residue. It requires a clean wipe to see some. This flux is alcohol-based no clean with 2% resin as solid content. I am used to using alcohol-based no clean with organic chemistry as flux activator and didn't have any issue with white flux residue build-up. J-STD-004 calls out four classifications of flux composition (Rosin/Resin/Organic/Inorganic). Is white powdery residue build-up from resin formulation in the flux we are using? any thoughts? thanks Matthew S. Park Preco Electronics tel: (309)-263-7788 fax: (309)-266-6674 1651 N. Main Morton. IL 61550 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------