TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Ken Bloomquist <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>
Date:
Mon, 28 Apr 2008 13:57:28 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (26 lines)
Further support for Werner's theory and probable root cause;

We never use to have this problem. We use to use chip bonder for the
secondary side SMD and wave solder them. We are now using selective pallets
which protects all the SMD parts from the wave solder and also protects them
from a lot of the bottom side preheat. The tiny ceramic cap is not getting
heated like the big honking connector stud. Bango the TCE cracks the cap!

I believe we've found the root cause now for corrective action. Let the
wheels start turning all you process genius' out there!

Thanks,

KennyB


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2