Mixing conformal coat (Acrylic and silicone) are scary business, unless
you have done good evaluation study about the combination....

jk

>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of
>Charles Caswell
>Sent: Monday, August 11, 2003 12:51 PM
>To: [log in to unmask]
>Subject: Re: [TN] conformal coating of BGAs
>
>
>I have no experience with underfill and have only coated a few
>boards. A labor intensive method used by one of my customers
>is to mix a batch of acrylic CC with extra thinner, squirt it
>under the BGA with a syringe. Cure then seal the edges with
>silicone. Then remove the excess CC before spraying.
>
>-----Original Message-----
>From: Collins Graham [mailto:[log in to unmask]]
>Sent: Monday, August 11, 2003 11:17 AM
>To: [log in to unmask]
>Subject: Re: [TN] conformal coating of BGAs
>
>
>Hi Joe!
>Well, as Joyce observed, Parylene will coat everything, so that's one
>(expensive) way.  Another way is to underfill the BGA before
>coating, with an underfill material.  This is what we are
>currently doing.
>
>I do question the ability of anyone to truly meet that
>requirement though, when using a conventional spray technique.
> For example, if you have vias under components (which is
>pretty much standard these days) then you will have exposed
>circuitry unless you are using a dry film solder mask.
>
>regards,
>
>Graham Collins
>Process Engineer,
>Northrop Grumman Canada Corporation
>Halifax
>(902) 873-2000 ext 6215
>
>>>> [log in to unmask] 08/08/03 03:04PM >>>
>Tech Netters,
>
>I am looking for some input on a special issue related to the
>conformal coating of boards with BGAs.  According to
>IPC-A-610C, section 9.1.2, voids in the conformal coating
>material can not expose circuitry, bridge lands or adjacent
>conductors.  In order words, all exposed circuitry/conductors
>are to be conformally coated.
>
>BGAs have conductors/solder balls located "under" the package
>unlike leaded parts where the leads are exposed and easily
>covered with conformal coating material.  Conformal coating
>may partially wick under the BGA covering some of the
>conductors/balls but not all the way. Some of the BGAs also
>stand off the board a measurable distance which the conformal
>coat material may not bridge resulting in an uncoated gap
>between the BGA and the pwb.  Some would interpret this as
>leaving exposed conductors (under the BGA).
>
>I would like to know how other manufacturers are dealing with
>this issue. Ideally, one would seal the perimeter of the BGA
>with conformal coat thereby not exposing conductors but
>conformal coat material will not bridge gaps greater than x
>mils.  Look forward to your response.  thanks
>
>joe
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/html/forum.htm for additional information, or contact
Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2