Hello,
Can anyone tell me the names of manufacturers with copper thickness
gauges capable of measuring copper clad/plate (0 - .004") on base
laminate thicknesses from 3 mils to 25 mils (.003" - .025")?
Thanks,
Annmarie Rainford
Merix Corporation
Forest Grove, Oregon.
503-359-9300
[log in to unmask]
|
|
|