TECHNET Archives

October 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Deac Descoteaux <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Deac Descoteaux <[log in to unmask]>
Date:
Tue, 21 Oct 2008 11:27:35 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (60 lines)
JOHN,

It sounds like double talk to me. It's either lead free or it AIN'T!!!!!!!!!

Deac 


Deac Descoteaux
PalPilot, East Coast
71 Spitbrook Road, Suite #307
Nashua, NH 03060
Cell# (603) 557-7568
Car# (603) 540-4173
Email: [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Foster
Sent: Tuesday, October 21, 2008 11:21 AM
To: [log in to unmask]
Subject: [TN] Lead Free BGA'S

Our assembly house recently assembled some boards with Lead Free BGA's for
us and when I asked them if they used a lead free process they responded
with.

We use leaded solder (Sn63Pb37) with a hybrid oven profile to accommodate
the lead-free BGA. I hope this answers your question. Please let me know if
you have any more questions."
Is this a common process, is this a reliable process

Any input is appreciated

Thank You
John Foster


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2