most likely yes. the msds of one of the wiper showed some of the content.
you need to find out exactly which one you use ;-).
http://msds-data.com/MSDS/Clorox/Clorox_Disinfecting_Wipe_Lemon_15948_msds.pdf
jk
> If Chlorox really does contain ionic chlorides and they are not removed
> then
> they could contribute to static dissipation on testing. That would make
> your
> tests somewhat false.
>
> --
> Regards
>
> Mike
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Louis Hart
> Sent: Wednesday, October 21, 2015 1:13 PM
> To: [log in to unmask]
> Subject: Re: [TN] ESD concern
>
> The people who make the mats must have some recommended or approved
> cleaner.
> Following up on Ioan's comment, chlorine can diffuse through the seal of
> an
> aluminum electrolytic capacitor and corrode the electrodes and
> connections.
> The chlorine is not consumed in the reaction, so the smallest amount will
> eventually destroy the part. Louis Hart
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Sue Powers-Hartman
> Sent: Tuesday, October 20, 2015 6:57 PM
> To: [log in to unmask]
> Subject: [TN] ESD concern
>
> We usually clean the ESD work tables with a product called Reztore. Now
> some employees feel that this product is not getting the tables clean
> enough
> so they are using Clorox wipes. Will this strip the ESD properties from
> the
> table top? If they use the Clorox wipes and then come after and wipe down
> with Reztore, would that be acceptable.
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|