Eric,
There is not a good metallurgical difference between soldering and
brazing except for temperature. Brazes typically melt at higher
temperatures than solders. But I'm sure there is some overlap between
the two.
mark
Mark Woolley
PTRL Laboratory
Avaya, 1300 West 120th Ave, Area 33, Westminster, CO, 80234
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
Sent: Monday, October 13, 2008 2:50 AM
To: [log in to unmask]
Subject: Re: [TN] Need soldering advice ASAP No II - tangential
question..
Interesting post Mike,
At the risk of going a little off topic I've never quite understood the
distinction between a solder and a braze. Is there a clear cut
difference in the metallurgy of the different joints?
Regards,
> The usual wisdom on soft solders is that they aren't very strong, so
the
> more ductile the alloy the less likely it is to break. This
conventional
> wisdom doesn't really apply to Au/Sn as it is more like a braze with
tensile
> and sheer about 8x 10x lead alloys.
>
--
Eric Christison Msc
Mechanical Engineer
Consumer & Micro group
Imaging Division
STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom
Tel: +44 (0)131 336 6165
Fax: + 44 (0)131 336 6001
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|