Sounds like moisture entrapment to me. A little moisture, some heat....
steam... and pop!! What temperature and how long do you bake the boards?
Were they soldered shortly after bake?
Gerry S.
----- Original Message -----
From: Stephen R. Gregory <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, August 28, 1999 10:37 AM
Subject: [TN] Blisters or Delamination after Wave...
> Hi ya'll!
>
> Well, I'm in onna Saturday...(Months end, you know how that goes!). Just
> finished waving a small lot of boards (9 assemblies) and 5 of them came
off
> the wave with these dime to quarter-sized delaminated blisters, maybe 3-4
of
> them on each board, and the other 4 boards looked fine! What would cause
> that? Entrapped moisture? The boards were supposedly baked before wave (At
> least the traveler said they were). Any ideas?
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|