18% solids is no problem. I'm spray fluxing an OA with 25% solids using
the Vitronics-Soltec. I'm getting very good hole fill on boards up to
.150" thick.
Give me a call if you need more info.
Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
500 Riverpark Drive
North Reading, MA 01864
Tel: 978-370-1726
(Embedded
image moved TechNet <[log in to unmask]>
to file: 08/20/2001 04:06 PM
pic05233.pcx)
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Spray Fluxer
Technetters,
Need to know if there is anyone that uses OA flux in a Spray Fluxer for
wavesoldering. Let me know if I can contact you off line to discuss some
general questions. I am being informed that there is not one single spray
fluxer out there that will handle OA flux due to its high (18%) solids
content. I need to know if this is true.
ARWBA. Thanks.
Bill Kasprzak
Moog Inc., Electronic Assembly Engineering
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|