TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Mark Hargreaves <[log in to unmask]>
Date:
Wed, 14 May 2003 15:36:44 -0400
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Mark Hargreaves <[log in to unmask]>
Parts/Attachments:
text/plain (100 lines)
Additional Comment-

IPC-4101 sheet 24 is a higher temp FR4 spec (Tg minimum 150 C).
In addition, the spec sheet for the FR4 we use indicates "typical Tg" of 175
C, which equals the rating of your component.



Mark



        -----Original Message-----
        From:   Mark Hargreaves [SMTP:[log in to unmask]]
        Sent:   Wednesday, May 14, 2003 2:59 PM
        To:     [log in to unmask]
        Subject:        Re: [TN] Hot Boards!

        Carl and Mike,
        Far as I know, 130 C is the highest continuous operating temperature
rating
        that UL will give any FR4 material.

        Regards,
        Mark


                -----Original Message-----
                From:   Mcmaster, Michael [SMTP:[log in to unmask]]
                Sent:   Wednesday, May 14, 2003 2:30 PM
                To:     [log in to unmask]
                Subject:        Re: [TN] Hot Boards!

                Carl

                You got the 120C number from Table 4-1 in IPC-2222, right?
What's
        the minimum dielectric thickness in the board?  It's also important
to note
        that this chart just lists FR4 and doesn't have a separate listing
for
        Higher Tg materials.   I think this is why they include footnote 6
"Other
        materials in the same classification with higher operating
temperatures may
        be available."  You want to avoid low Tg FR4 materials since you'll
be very
        close to that transition point.  The best thing to do is find out
from the
        laminate manufacturer what the maximum continuous operating
temperature for
        their material is.  This information is not usually on the standard
data
        sheets but it is available.

                One other thing you need to watch out for is to make sure
you're
        fabricator has UL recognition for high enough Maximum Operating
Temperature
        (MOT) for the materials used in this board.  It's not enough to ask
for
        flammability.  You also need to specify a specific MOT if you want
it and
        you probably want at least 130C for this board.

                Mike McMaster
                RF Product Engineer
                Merix Corporation
                503-992-4263


        ---------------------------------------------------
        Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
        To unsubscribe, send a message to [log in to unmask] with following
text in
        the BODY (NOT the subject field): SIGNOFF Technet
        To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
        To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
        Search the archives of previous posts at:
http://listserv.ipc.org/archives
        Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
        information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
        -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2