Additional Comment- IPC-4101 sheet 24 is a higher temp FR4 spec (Tg minimum 150 C). In addition, the spec sheet for the FR4 we use indicates "typical Tg" of 175 C, which equals the rating of your component. Mark -----Original Message----- From: Mark Hargreaves [SMTP:[log in to unmask]] Sent: Wednesday, May 14, 2003 2:59 PM To: [log in to unmask] Subject: Re: [TN] Hot Boards! Carl and Mike, Far as I know, 130 C is the highest continuous operating temperature rating that UL will give any FR4 material. Regards, Mark -----Original Message----- From: Mcmaster, Michael [SMTP:[log in to unmask]] Sent: Wednesday, May 14, 2003 2:30 PM To: [log in to unmask] Subject: Re: [TN] Hot Boards! Carl You got the 120C number from Table 4-1 in IPC-2222, right? What's the minimum dielectric thickness in the board? It's also important to note that this chart just lists FR4 and doesn't have a separate listing for Higher Tg materials. I think this is why they include footnote 6 "Other materials in the same classification with higher operating temperatures may be available." You want to avoid low Tg FR4 materials since you'll be very close to that transition point. The best thing to do is find out from the laminate manufacturer what the maximum continuous operating temperature for their material is. This information is not usually on the standard data sheets but it is available. One other thing you need to watch out for is to make sure you're fabricator has UL recognition for high enough Maximum Operating Temperature (MOT) for the materials used in this board. It's not enough to ask for flammability. You also need to specify a specific MOT if you want it and you probably want at least 130C for this board. Mike McMaster RF Product Engineer Merix Corporation 503-992-4263 --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 -----------------------------------------------------