Genny,
I'd scrap it, depending upon your product reliability requirements. If you're doing inexpensive radios or the such, check the viscosity, and if within spec, run 30 boards and check the results. You can then form your opinion from there.
Lunch in the paste fridge? Our firm would fire the entire staff!
Leland
________________________________
From: TechNet on behalf of Genny Gibbard
Sent: Fri 2/9/2007 10:25 AM
To: [log in to unmask]
Subject: [TN] What to do with expired solder paste?
Was sorting through the fridge in the stockroom at work...pushed aside a
couple of sandwiches and yogurts (the stockroom people keep their
lunches in there...) and came across a box with 9kg(18 jars) of solder
paste expired in mid 2004 - a brand we don't use any more. Standard
63/37 no-clean.
What would you do with it? Never even been opened.
Genny.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|