Barbara-
Lots of good feedback already on this post. Just want to stress that the
environment your assembly is in will be VERY important. We coat most
everything (automotive) and the coating used is usually a compromise of
what the application can live with and what the CEM is willing to put in
their equipment. We've seen silicone coatings introduce problems over time
due to outgasses from the coating reacting with other materials in the
overall assembly. Seen acrylic coatings that were eaten up by the type of
grease used elsewhere, etc., etc...
Best Regards and Good Luck,
-Chris
Barbara Burcham
<[log in to unmask]> To: [log in to unmask]
Sent by: TechNet cc:
<[log in to unmask]> Subject: [TN] Conformal Coating of
Assembled Boards
05/16/2005 05:55 PM
Please respond to TechNet
E-Mail Forum; Please
respond to Barbara Burcham
Well, my company now has an application requiring conformal coating on
some small assembled boards. We need to mask off 3 connectors and coat
everything else.
I have some information on a product called Parylene applied by Parylene
Coating Services, Inc. in Katy, Texas.
We did a small lot with a simple spray-on process, but that is not the
way to do production runs, of course.
What would you recommend?
Thanks,
Barbara
Barbara J. Burcham, C.I.D.
Fairfield Industries, Inc
281-275-7687
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This e-mail message is intended only for the use of the intended recipient(s). The information contained therein may be confidential or privileged, and its disclosure or reproduction is strictly prohibited. If you are not the intended recipient, please return it immediately to its sender at the above address and destroy it.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|