Dear Waleed,
Finished Thickness means overall thickness = total measured thickness (1.6
mm usual).
Unless it shows the question for Copper thickness, where it could mean Base
copper + plated copper.
Such as 17 metric microns + 25 metric microns = 42 metric microns (usual for
outer layers)
Very Best Regards
Roland
PCB Consultant - Company viability, Technical viability, Technology choice,
Yield improvement, Company Strategy, Equipment choice, Company acquisition
Roland Jaquet - Tel. +41-22-880-0405 - Fax. +41-22-880-0409 - Cell
+41-79-203-3723
http://www.PCBspecialist.com
_______________________________________________________________________
----- Original Message -----
From: Waleed Abdel-Hameed <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, September 25, 2000 7:17 AM
Subject: [TN] fab
> Dear all:
> What's a finished thickness.I need to make a RFQ any
one
> know a good pcb fab.
> Thank's
> waleed
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|