Dear Waleed, Finished Thickness means overall thickness = total measured thickness (1.6 mm usual). Unless it shows the question for Copper thickness, where it could mean Base copper + plated copper. Such as 17 metric microns + 25 metric microns = 42 metric microns (usual for outer layers) Very Best Regards Roland PCB Consultant - Company viability, Technical viability, Technology choice, Yield improvement, Company Strategy, Equipment choice, Company acquisition Roland Jaquet - Tel. +41-22-880-0405 - Fax. +41-22-880-0409 - Cell +41-79-203-3723 http://www.PCBspecialist.com _______________________________________________________________________ ----- Original Message ----- From: Waleed Abdel-Hameed <[log in to unmask]> To: <[log in to unmask]> Sent: Monday, September 25, 2000 7:17 AM Subject: [TN] fab > Dear all: > What's a finished thickness.I need to make a RFQ any one > know a good pcb fab. > Thank's > waleed > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################