Subject: RE: [TN] PCB delamination at area with ground-plane cutout [...][log in to unmask]
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask][log in to unmask]] On Behalf Of stephen gregory
Sent: Saturday, April 22, 2017 4:19 PM
To: [log in to unmask]
Subject: [TN] Removal from TechNet message?

Hi All,
Just curious, did anybody else get this message last night:
Sat, 22 Apr 2017 00:00:06 [...][log in to unmask]
Date:
Thu, 20 Apr 2017 15:33:40 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (42 lines)
Dell - Internal Use - Confidential  

I don't have a copy of F rev. only G rev.   What is the verbiage of this section.

Victor,

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
Sent: Thursday, April 20, 2017 10:13 AM
To: [log in to unmask]
Subject: Re: [TN] IPC Standard

IPC-A-610-F section 6.2.1.2 is probably transferable to terminating into a PCB directly. 

Ed Popielarski
Engineering Manager


                               970 NE 21st Ct.
                              Oak Harbor, Wa. 98277

                              Ph: 360-675-1322
                              Fx: 206-624-0695
                              Cl: 360-544-2289



       "It's one kind of victory to slay a beast, move a mountain, and cross a chasm, but it's another kind altogether to realize that the beast, the mountain, and the chasm were of your own design."
https://goo.gl/maps/mMjg43rXeFB2

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Thursday, April 20, 2017 8:01 AM
To: [log in to unmask]
Subject: [TN] IPC Standard

Fellow TechNetters:

    Is there a STANDARS for insulated wire cable soldering onto a PWB?   Is melted terminating insulation acceptable?