IPC-600-6012 Archives

January 2001

IPC-600-6012@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Les Hymes <[log in to unmask]>
Reply To:
Combined Forum of D-33a and 7-31a Subcommittees <[log in to unmask]>, Les Hymes <[log in to unmask]>
Date:
Tue, 23 Jan 2001 17:11:51 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (45 lines)
Looks "rough and frayed" at this mag to me.

Caveats would be
1) How does it look at the same mag as in -600F?  The mag on sample appears
to be significantly higher than pics from 600F

2) Does it impair form/fit/function - or might it.

3) Process Control or lack thereof?

Les Hymes
----- Original Message -----
From: John Perry <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, January 23, 2001 2:15 PM
Subject: [IPC-600-6012] Nonconforming Condition for Nonmetallic Burrs?


Hi All,


Got an issue here raised by one of our IPC-A-600F users.  The attached .pdf
contains a photograph that shows the board edge of a sample which the user
believes does not pass the criteria established in section 2.1.1.1.,
Nonmetallic Burrs.  It would appear as though the router had some problems
on the edges and fiberglass fibers are now falling off the edges.

Does this provide sufficient information in order to obtain a consensus from
this group on the pass/fail issue?


Best Regards,




John Perry