DESIGNERCOUNCIL Archives

1996

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vmOsJ-0000fZC; Mon, 20 Jan 97 12:55 CST
Content-Type:
TEXT/PLAIN; charset=US-ASCII
Old-Return-Path:
<bergda>
Date:
Mon, 20 Jan 1997 12:55:12 -0600 (CST)
Precedence:
list
Resent-From:
cc:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/2294
TO:
Mike Gnieski <[log in to unmask]>
Return-Path:
<DesignerCouncil-request>
From [log in to unmask] Tue Jan 21 12:
28:13 1997
X-Status:
Resent-Message-ID:
<"LhqKl1.0.EBH.K-xuo"@ipc>
Subject:
From:
David Bergman <[log in to unmask]>
X-Loop:
In-Reply-To:
Message-ID:
<Pine.3.89.9701201229.I71721-0100000@ipc>
Resent-Sender:
DesignerCouncil-request [log in to unmask]
Parts/Attachments:
TEXT/PLAIN (41 lines)
According to the IPC spex the total thickness would be over all metal 
including platings.

Regards
Dave Bergman IPC


On Mon, 20 Jan 1997, Mike Gnieski wrote:

> Could someone settle a debate? What is the
> correct measurement of the total thickness
> of a multilayer board, glass to glass or
> copper to copper?
> 
> thanks
> Mike Gnieski
> 
> ***************************************************************************
> *   The mail list is provided as a service by IPC using SmartList v3.05   *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to:           *
> * [log in to unmask] with <subject: unsubscribe> and no text.*
> ***************************************************************************
> * If you are having a problem with the DesignerCouncil, please contact    *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
> 
> 

***************************************************************************
*   The mail list is provided as a service by IPC using SmartList v3.05   *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.*
***************************************************************************
* If you are having a problem with the DesignerCouncil, please contact    *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2