According to the IPC spex the total thickness would be over all metal including platings. Regards Dave Bergman IPC On Mon, 20 Jan 1997, Mike Gnieski wrote: > Could someone settle a debate? What is the > correct measurement of the total thickness > of a multilayer board, glass to glass or > copper to copper? > > thanks > Mike Gnieski > > *************************************************************************** > * The mail list is provided as a service by IPC using SmartList v3.05 * > *************************************************************************** > * To unsubscribe from this list at any time, send a message to: * > * [log in to unmask] with <subject: unsubscribe> and no text.* > *************************************************************************** > * If you are having a problem with the DesignerCouncil, please contact * > * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * > *************************************************************************** > > *************************************************************************** * The mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To unsubscribe from this list at any time, send a message to: * * [log in to unmask] with <subject: unsubscribe> and no text.* *************************************************************************** * If you are having a problem with the DesignerCouncil, please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************