Another thing to note is Soldermask Inks have come along way.
What was being used at one time for bulk fillers and matting
agents has changed greatly to help with both solder balls and
SIR values.
Dave
-----Original Message-----
From: Don Vischulis [mailto:[log in to unmask]]
Sent: Thursday, October 14, 1999 4:52 PM
To: [log in to unmask]
Subject: Re: [TN] matte vrs gloss LPI
Rudy:
Won't take that bet, but my experience indicates that you'll see maybe a
decade lower
SIR value with a very matte mask versus a gloss or semi gloss after
identical
processing and cleaning. You'll also find that after wave solder, matte has
less
tendency to retain solder balls than gloss.
Any dispute?
Don Vischulis
Rudy Sedlak wrote:
> Have money in my pocket that says I can clean up matte soldermask so that
it
> will pass SIR.....
>
> Rudy Sedlak
> RD Chemical Company
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|