TECHNET Archives

October 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Fri, 8 Oct 1999 19:45:15 -0400
Content-Type:
text/plain; charset="us-ascii"
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, joyce <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Steve,
He is referring to a Manual bonder, not automatic wire bonder.  Manual
bonder has a simple position system and a handle to push for each bond...You
still need a machine (look like a sewing machine with wedge...nothing
fancy!) with optical microscope... by the way, if you really want to get
into the manual bonding business, you can talk to Palomar or K&S, they may
know who has some old manual bonder for sale...(you need some
training...take IMAPS tech course (at end of this month) about wire bonding
for a good start...The wire bonding god is teaching this fall..you are a
lucky chap if you go)...

check following web site for bonder infor and contact telephone numbers:

http://supersite.net/semin2/palomar/home.htm
http://www.kns.com/pro-8000.htm

Good luck for your diversification, multi-talent, increase responsibility,
flexibility, etc.etc. (mention it to your sales guy..there is a price tag
associated to get into even "manual bonding"...He may back it down..).

may god be with you this time too...
                                  joyce

At 03:37 PM 10/8/99 EDT, you wrote:
>Hi ya'll...
>
>I gotta silly question, can wire bonding be done by hand? We've got a sales
>guy that's trying to drum up some business for us, call me last week and
>asked if we had the capability to do wire bonding here. I told him no-way,
>don't have a wire bonding machine here, and that we weren't really set-up to
>do something like that here anyway.
>
>Well he calls again today, and said that he understands that we don't have an
>automated wire bonder, but the potential customer said that the volume that
>they were looking at, it should be something that we could do by hand. I
>said; "WHAT? Wire bond by hand? NO-WAY!" I think our sales guy understood
>"manual" wire bonding, to mean "by hand" like you would hand solder a
>component. I did a NET search and found a lot of manual wire bonding stations
>but they were pretty sophisticated looking machines...nothing about wire
>bonding by "hand" though. Sorry about the dumb question...
>
>-Steve Gregory-
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2