In a message dated 09/03/1999 10:52:48 AM Central Daylight Time,
[log in to unmask] writes:
<< Steve,
30% concentration of Kyzen? Is this stuff pre-diluted?
It is my experience that good cleaning will result at concentrations of less
than 10%. Most folks I know would prefer to run at less than 5%, 'cos it
costs less - but 30%??
Please enlighten me or have I missed the plot.....
Regards,
Graham Naisbitt
[log in to unmask] >>
Hi Graham!
No that's a 30% concentration, I measure it with a refractometer. Here's why
the 30%; currently for the mil-spec SMT stuff they've been running a no-clean
paste and have to clean the residues...(I know what you're thinking) believe
you me, the next thing on my list is to get an RMA paste in here...(only got
so many hours in a day and can only fight so many fires at a time) ANYWAYS,
if the concentration gets into the 20's there's a white residue that
results...can't have that around here. (gawd, I'm looking forward to this
3-day weekend!)
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|