Rod Semen wrote:
>
> I recently was told that Bellcore has not approved any of the alternative
> oxide processes out there. Could anyone elaborate on this?
>
> ______________________________________________________
> Get Your Private, Free Email at http://www.hotmail.com
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
That is not true! Around September 25, 1999, McGean-Rohco received
Telcordia (Bellcore) approval for the DuraBOND Multilayer bonding system
(white oxide). This is the only Bellcore approved oxide alternative in
the field (We have the Technology and Reliability report to prove it!).
If you need more information call (216)441-4900.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|