Uday,
I've successfully avoided bridging on these connectors in the past
by using "paint dams" around the connector lands in addition to
thieving pads at the trailing edge. Just add a rectangular paint
area under the connector on the solder wave side legend with openings
for the lands the same size as your soldermask reliefs (assuming this
leaves a web of paint between each land.) However, I also always have
been able to orient the connector placement so the rows ran perpendicular
to the wave & not parallel and I believe (if I understand your orientation
relative
to the wave correctly) running with the rows parallel to the wave is the
most
significant cause of your bridging.
Tom Martin
Sr. PCB Designer
ASE Technologies USA
Date: Thu, 12 Aug 1999 15:25:46 -0700
From: "Uday V. Putcha" <[log in to unmask]>
Subject: 50-mil pitch two row connectors
MIME-Version: 1.0
Content-Type: text/plain; charset="us-ascii"
Hello All
We have 50-mil pitch two row TH connectors on some of our boards. The
direction of flow in wave is parallel to the row of pins. This part always
bridges on the last pins as there is lot of drag at the end. We also tried
to add a thieving pad at the end of the last pin in the direction of flow
to help, but the test results didn't help much. (only 50% yield).
Does anyone has experience with this case? Any help is appreciated
Thanks
Uday
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|