TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
David Hillman <[log in to unmask]>
Date:
Tue, 31 Aug 1999 12:19:43 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Nick D'Onofrio <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (63 lines)
Hi Nick - take a look at the TechNet archives - there has been several good
threads that contain the answers you are looking for! Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




"Nick D'Onofrio" <[log in to unmask]> on 08/31/99 08:26:24 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to "Nick D'Onofrio" <[log in to unmask]>

To:   [log in to unmask]
cc:
Subject:  [TN] Pre-tinning gold leads




  We are pre-tinning the gold leads prior to assembly on our military
products. I'm looking for some constructive data or argument to decide if
we
should continue this practice.
  My concern would be gold embrittlement in the solder joint and any latent
failures attributed to this.
  Any comments or guidance in this matter would appreciated.

Regards,
Nick D.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2