I guess you had better to look over the category QMFZ2 also, in addition
to ZPMV2
Toru Koizumi
Fujikura Ltd.
>Don,
>
> Thanks for the info, it was helpful. I couldn't get have got it
>quicker anywhere else. Just shows how useful TechNet is.
>
>> Geoff Layhe
>> > Lamar-UK Ltd
> > www.lamar-uk.co.uk
>
>> ----------
>> From: Don Vischulis[SMTP:[log in to unmask]]
>> Reply To: TechNet E-Mail Forum.;Don Vischulis
>> Sent: 25 August 1999 22:47
>> To: [log in to unmask]
>> Subject: Re: [TN] UL Approval.
>>
>> Geoff:
>>
>> ZMP-V2 is a section in the UL recognized components directory either
>> where printed
>> wiring boards or plastic laminates are listed. (I'm not certain
since
>> I'm typing this
>> from home, but the heading for the two sections are similar.) My
>> interpretation of
>> your requirement is that the specification is looking for a UL
>> recognized material.
>> Most commercial laminates have been evaluated by UL and the file
>> numbers may be
>> obtained from the manufacturer.
>>
>> From your web page, I notice that you are a distributor of ISOLA
>> laminates. Most if
>> not all of the laminates manufactured by ISOLA USA are UL recognized
>> components. (This
>> is also true of other laminate manufacturers.)
>>
>> Don Vischulis
>> [log in to unmask]
>>
>> Geoff Layhe wrote:
>>
>> > Hi All,
>> >
>> > Can anybody help with a UL material reference?
>> > I have been asked to specify a copper clad laminate which is "a UL
>> > recognised material suitable for live parts to ZPM-V2". The
laminate
>> is
>> > for a circuit board in a control system.
>> > The only UL specs I've seen for laminates are UL 796 & UL 94 &
these
>> > don't mention ZPM-V2.
>> >
>> > Anybody come across this reference before?.
>> >
>> > Geoff Layhe
>> > Lamar-UK Ltd
>> > www.lamar-uk.co.uk
>>
>> ##############################################################
>> TechNet Mail List provided as a free service by IPC using LISTSERV
>> 1.8c
>> ##############################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>> following text in
>> the body:
>> To subscribe: SUBSCRIBE TECHNET <your full name>
>> To unsubscribe: SIGNOFF TECHNET
>> ##############################################################
>> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>> additional
>> information.
>> If you need assistance - contact Gayatri Sardeshpande at
>> [log in to unmask] or
>> 847-509-9700 ext.5365
>> ##############################################################
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
or
>847-509-9700 ext.5365
>##############################################################
>
----
Fujikura Ltd. [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|