TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 26 Aug 1999 15:52:11 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
"Stephen R. Gregory" <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
In a message dated 08/26/1999 12:43:38 PM Central Daylight Time,
[log in to unmask] writes:

<< I am also dealing with LCC's (tiny MMICS) and have
 to put them down on a ground plane.  Do not want to
 turn the bottom into a BGA.  Are there any other ways
 to mount them? This is a (6) layer Rogers material board
 and there is an active plane on the bottom.
 You seem to have experience in this area.
 thanx.. >>

Hi ya!

If you go to: http://www.nasinterplex.com
It's a company that makes solder-bearing lead frames that you can mount to
the LCC's and give it more compliance...might have what you need. The
foot-print would be more of a "J" leaded PLCC footprint...

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2