Hello,
We use a chemical called Humiseal 1030 to remove conformal coating. It works well for us on any type of boards.
/Cecilia Alkhagen
-----Original Message-----
From: Hinners Hans CIV WRALC/LYPME [mailto:[log in to unmask]]
Sent: Thursday, August 26, 1999 3:04 PM
To: [log in to unmask]
Subject: [TN] Acrylic Conformal Remover which doesn't touch Epoxy? -
Does it e xist
Hey Everybody,
I'm looking for an acrylic conformal coating remover which won't touch
epoxy.
I tried Kyzen's Conformox AU and it changed the physical appearance of the
epoxy - dulled it.
I should run a hardness test but I think it softened it too.
The current plan uses Trans LC and that leaves a hazy residue.
This residue does come off when I run it through our Aqueous Cleaner or get
the q-tips out but . . .
an extended soak in Trans LC will soften the epoxy too, so I'm highly
motivated to find an alternative.
I'm not familiar enough with the properties of acrylic and epoxy to know
whether I'm trying to defy physics (yet!).
Somebody out there in cyberland must have faced this opportunity already.
Hans
5 more days and I will have been in the Industry for 1 whole year.
Air Force Material Command
Our mission: develop, deliver and sustain the best products for the world's
best Air Force.
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|