Hans,
One place to check is ACS (Advanced Chemill Systems). They are not cheap and they don't have the greatest field service, but they do build to spec, very specialized, completely custom conveyorized dryers. Be sure to include all possible problems you forsee in drying the panel thickness range you are looking for. They are somewhere out in CA. Hope this is useful.
Most people are running automated hoist lines for oxide, and dryer noise is the least of their worries. They are just using a heated, forced air, full basket dryer. Of course drying times are longer than a conveyorized application.
Joe Aronson
Wet Process Engineer
JMSPI
>>> Hinners Hans CIV WRALC/LYPME <[log in to unmask]> 08/17/99 10:44AM >>>
Hi All,
I'm looking for recommendations on board dryers.
We do thin inner layers and flex (a couple of mils) through pretty thick
multilayered boards say ~150 mils.
I'm very interested in quiet. The ones we have now can be heard from
several hallways away and ear protection is required if you are in the room.
What do folks use to dry oxided panels?
Hans
Air Force Material Command - We keep them flying!
~~~~~~~~
Hans M. Hinners WR-ALC/LYPME Bldg. 640
Materials Engineer 380 Second Street,
Suite 104
Manufacturing Eng. Sec. Robins AFB GA 31098-1638
912-926-1970 (Voice) 468 - 1970 (DSN) 912-926-7974 (Fax)
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|