Good to hear you Kathy ; be it sad issues .
Pity Steve's not yet fully on line ; he'd tell you better than me :
Been there ; done that .
Trouble is Kathy ; yo're both right :
Your tech sense on clear test result gives clear verdict : fail
Purchasing knows if they knock back the boards/order/etc.
they will quite likely not see the customer again = their view : fail
When sandwiched in past: I enclosed all tests (wetability, vibrational if
requested, etc.) .
Just cover yours by proper documentation :
Did the test ; informed client of ramifications ; ask him if they want it
followed by vibration or shock test (no time for cycling) they would pay for
obviously ; inform them on warranty ramifications of all of this mess ,
and than sleep in peace .
Communicate ; I know sensistivity lessons sound strange from me ;
but believe me, when required, we should all be gentle, on ourselves as well
:
Where I came from the saying goes :
Loosing health for "limitations" of others does make you the same .
Cheers paul
PS
Aspirin ?
-----Original Message-----
From: Kathy Palumbo [mailto:[log in to unmask]]
Sent: Thursday, 29 July 1999 5:45
To: [log in to unmask]
Subject: Re: [TN] Dewetting Issues
FYI
They (purchasing) did not believe the solderability testing so they had us
build up boards anyway. When the boards passed test they said there was no
problem with the boards.
We all know this is not accurrate, because if you put enough solder down you
can mask off just about any dewetting problem out there.
Believe me I have already pondered the worse case senerio!
Regards,
Kathy Palumbo
-----Original Message-----
From: Franklin [mailto:[log in to unmask]]
Sent: Wednesday, July 28, 1999 12:20 PM
To: [log in to unmask]
Subject: Re: [TN] Dewetting Issues
Kathy,
Why would you be concerned with 'long term solderability' issues when you
have this initial solderability condition to deal with? Seems to me the
argument should be the 'here and now', and not the 'what if'.
All I know about reliability studies are those I have first hand experience
with, and that being as I wrote above, if they fail from the beginning, they
will not get any better sitting on a shelf.
<smile> Something to ponder.
Franklin D Asbell, CQA
Network Circuits, Inc.
Irving, Texas
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|