Hi Gendelis! I suggest you try either Alpha, Kester, Multicore, or Indium
as first possible sources - your solder alloy is very nontypical so don't
be surprised if no one has it or you have to pay a premium to get it. A
second possible source is Arconium Specialty Alloys  (1-800-343-0282) -
they do not list the Bi52/Pb48 alloy but they do list a 58Bi/42Pb in their
products list. What is the intended application for the alloy? Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Gendelis Haviv <[log in to unmask]> on 05/04/99 10:35:28 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to Gendelis Haviv <[log in to unmask]>

To:   [log in to unmask]
cc:
Subject:  [TN] Bi52Pb48




Dear technetters!

Does anyone know a source for solder wire Bi52Pb48?


Gendelis Haviv
Process Engineer
ECI TELECOM

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2