There was a great report put out by I think Ames , or Langley , (it was
listed in NASA tech briefs) that discussed the pyrolysis of Polyimides ,
I might have a copy , I'll check
Russ
----------
From: Alderete, Michael
To: [log in to unmask]
Subject: [TN] FW: re Polyimide, temperature for discoloration and /or
pyrolosis [charring]
Date: Wednesday, May 19, 1999 2:30PM
rejected [why??}, and resending message below
-----Original Message-----
From: Alderete, Michael
Sent: Wednesday, May 19, 1999 11:24 AM
To: 'IPCtechnet'
Subject: Polyimide, temperature for discoloration and /or pyrolosis
[charring]
Help.
Anyone know what temperature polyimide [in PWB]:
a. starts to discolor
b. pyrolizes, or chars?
Had similar problem at the last company- 3 phase power, 115V AC, runs
into
rig-flex backplanes on F/A-18 targeting pod. Water [salt water or wash
down
fluids] was getting into vented elec boxes, and shorting out the 3 phase
power. Fire and black stuff all over inside of box resulted.
Know very little about current design and circumstances, but our guys
think
it's a short induced problem. PI material darkens; don't think they see
charring in this instance.
Thanks in advance
Michael
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
|