Hi Neil,
TLC-32 is a glass reinforced PTFE substrate material made by Taconic
Advanced Dielectric Division in Petersburgh, NY. Their phone number
is 1-800-833-1805.
Hope this helps...Andy
______________________________ Reply Separator _________________________________
Subject: [TN] What the hell is this stuff??
Author: Neil Atkinson <[log in to unmask]> at smtplink-hadco
Date: 05/14/99 12:17 PM
We've just received a drawing that quotes a spec for laminate which no one
seems to recognise, can anyone tell me what it is.
The material is quoted as: TLC TAC-LAM (32-0310-CH/CH) SUBSTRATE 31 THOU
THICK. DIELECTRIC CONSTANT 3.2 1/2 OZ ELECTRO-DEPOSITED COPPER BOTH SIDES.
Thanks,
Neil
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|