Jim: Since you didn't state what it is you are trying to measure or the
resolution required I can't give you an exact instrument type. However if you
are trying to measure such things as polymer thick film or soldermask thickness
and/or topography; or all the way down to things like copper surface roughness
or scrub patterns, I would contact: Tencor Instruments Metrology Div. Santa
Clara Ca. 408-970-9500. They make a wide variety of surface profiling and
measurement instrumentation.
Regards
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett Wa.
425-356-6076
Does anyone one out there know of a gauge that can be run over the =
surface of a product and record the lowest and highest point. We have =
these with dials you can watch but I'm not aware of one that can =
"record" the extremes.
Thanks,
Jim Gleason
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################