Hi Earl,
I'm certainly no expert on metallurgy, but I have learned a bit. Well
so much for joining without diffusion. Some of these metals are going to
diffuse even at room temperature over time. The room temperature of tin/copper
at room temperature is well known. I havent looked at lead per se', but I
suspect that it will diffuse also, perhaps at a slower rate. I'll leave further
discussions up to the metallurgists.
Keep your Nose on the horizon !!
Les
> From: [log in to unmask], on 2/9/99 5:07 PM:
> Phil and everyone,
>
> I have difficulty shaking Dr. Manko's old definition (as Werner so astutely
> pointed out) soldering
> is the joining of two metal surfaces, using a solder medium, without
> requiring diffusion or
> intermetallic formation. I recoginze we've come far since this time.
> However, I must ask is it
> possible to solder two metals (only their surfaces) without forming
> intermetallics, at least
> initially, under any condition short of time not being a factor?
>
> Earl Moon
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|