Earl,
I do not concur with the definition as described. I firmly believe, and
teach, that the definition of soldering must include the creation of
intermetallics, at least in the case of Sn/Pb and copper substrates.
Logically I expect it will extend to other materials as well, due to the
fundamental nature of the wetting and intermetallic formation mechanism.
I offer as evidence, a statement I usually make to the folks I am
instructing:
It is accepted that it is a common occurrence that copper will diffuse into
a working solder bath as a product of exposure to the copper substrate.
Show me a bath that is not accruing copper, and I will show you exposed
copper areas!
Am I wet (with solder) behind my ears?
JMW
TET/Halco
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|