I am having a problem with inspection of the above mentioned subject, My
branch has contracted to build the end item product for NAVSEA, The supplier
of the circuit cards sub-contracted the building of same. I have been doing
incoming inspection of the circuit cards and found numerous defects in the
area of side overhang exceeding 25% of the component pad. This area has
irritated the supplier to say the least, and has responded by saying that
the only inspection criteria that I can now use is by inspecting the leads
from the toe end of the leads,straight on and not from a top view that is
required because of the enourmous amount of surface mount components. The
inspection criteria for these circuit cards is per IPC-610, class 3, High
Performance Products. My question to you, "Is this the only way that I am
allowed to inspect the leads or am I allowed to inspect them from all angles
if necessary ?" and is this process documented in IPC-610 anywhere? Because
I can't seem to find it anywhere between the covers of the manual.
Lonnie Brinson
Code 6072
Bldg 2930
854-2301
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|