Hi Paul:
Sometimes an uncured or improperly cured soldermask can cause whitish
residue on the sides that are exposed to heat such as wave solder
process.
Chetan
>Date: Fri, 15 Jan 1999 17:04:48 -0400
>Reply-To: "TechNet E-Mail Forum." <[log in to unmask]>,
> Paul Wareham <[log in to unmask]>
>From: Paul Wareham <[log in to unmask]>
>Subject: [TN] White blistering on solder mask.
>To: [log in to unmask]
>
>Getting alot of white blister marks on a batch of boards. All boards =
>seem to be from the same date code of board manufacture. The marks
seem =
>to occur over all areas, not just over copper. There is no residue and
=
>does not scrape, it looks like it is subsurface. To me, it looks as =
>though there is some weakness in the solder mask which was brought out
=
>under the stress of wave solder. The marks are only on the solder
side, =
>and only seem to appear after they've been washed. Could a defective =
>solder mask have been damaged by heat stress of the wave, then
providing =
>a home from moisture during the wash process?
>
>Any ideas?
>
>Paul Wareham
>DynaGen Systems Inc.
>
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|