Ironically, I had engineers from Insulfab in-house last week. I'm
evaluating composite solder pallets as an alternative to our current
anodized aluminum pallets. The technical support from a materials and
mechanical engineering standpoint is very good. The prices are also very
competitive.
----------
> From: Jim Gleason <[log in to unmask]>
> To: [log in to unmask]
> Subject: Re: [TN] Wave Solder Fixtures
> Date: Friday, November 06, 1998 5:26 PM
>
> Try GSC at www.goGSC.com. I think they are about the best around.
>
>
> ----------
> > From: Reginald Swipe <[log in to unmask]>
> > To: [log in to unmask]
> > Subject: [TN] Wave Solder Fixtures
> > Date: Friday, November 06, 1998 3:41 PM
> >
> > Hi Technetters,
> >
> > Please can somebody advise me about good suppliers of Wave Solder
> > pallets. In particular a new outfit called Insulfab have arrived on the
> > scene. Has anyone used them? Do they do a good job? Any feedback would
> > be appreciated.
> > Thanks,
> > Reggie
> >
> > ______________________________________________________
> > Get Your Private, Free Email at http://www.hotmail.com
> >
> > ################################################################
> > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> > ################################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> > To subscribe: SUBSCRIBE TechNet <your full name>
> > To unsubscribe: SIGNOFF TechNet
> > ################################################################
> > Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> > For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> > ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|