Fellow Technetters,
Does anyone out there have any good comparisons or stories about some of the new
solders on the market. I have been approached and am evaluating a couple of
different solders. I'm trying to see what the "long term" benefits would be.
Extra pure solders 4-9's are good for how long before you get what you had in
the first place? Phosphorous added solders are good for how long? Benefits,
downfalls??? They all offer a good deal to switch and back with a guarantee in
the initial stages in defect reductions and dross generations, but where will I
be a year from now? I currently use a standard grade of 63/37. Can anyone shed
any light on my delima?
Jason Smith
Lexmark Electronics
Process Materials Engineer
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|