TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
"<Jason M. Smith>" <[log in to unmask]>
Date:
Fri, 20 Nov 1998 07:44:32 -0500
Content-Type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (27 lines)
Fellow Technetters,
Does anyone out there have any good comparisons or stories about some of the new
solders on the market.  I have been approached and am evaluating a couple of
different solders.  I'm trying to see what the "long term" benefits would be.
Extra pure solders 4-9's are good for how long before you get what you had in
the first place?  Phosphorous added solders are good for how long?  Benefits,
downfalls???  They all offer a good deal to switch and back with a guarantee in
the initial stages in defect reductions and dross generations, but where will I
be a year from now?  I currently use a standard grade of 63/37.  Can anyone shed
any light on my delima?

Jason Smith
Lexmark Electronics
Process Materials Engineer

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2