Hi Tim,
Yes, we have tried that approach ....we even have made some of our designs like
that at your facility.... the olnly issue there is the additional standoff,
especially that close to the BGA pads and less than 0.025" SMT ...that
definitely affects the solder print resolution/process....let me know if you can
think of any other 'relatively inexpensive' way of doing this....
Marcelo
-----Original Message-----
From: Tim Snodgrass [SMTP:[log in to unmask]]
Sent: Thursday, October 22, 1998 6:12 PM
To: TechNet E-Mail Forum.; Chan, Marcelo
Subject: Re: [TN] Plugged/tented vias
Marcelo
We have used a two step soldermask process to tent vias. First we put a
layer of dryfilm down and print it
with via image. Then coat the board with liquid soldermask. Then print
that image. This produces a part
with tinted via's and liquid photoimageable to ensure that there is no
entrapment in the via holes. If you
have any questions contact me off line.
Regards,
Tim Snodgrass
Young Electronics
818 407-4024
Chan, Marcelo wrote:
> We have tried different approaches to tenting/plugging vias for BGA
and some
> backplane applications using LPI and screened SM with limited
success...PWB
> vendors claim they could do it, but we are still looking for some one
who could
> do this on 100% of the vias with no pin holes and it has to be done on
both
> sides to prevent entrapment of cleaning solutions...the via sizes that
we have
> in mind can have a finished hole diameter as large as 22 and as small
as 13
> mils...Can someone share their 'hands-on' experiences on this issue
with me
> through Technet or even off-line?
> Thanks
>
> Marcelo Chan
> Lead Engineer - Advanced Manufacturing Technology
> Electronics Systems Sector, Harris Corp., FL
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|