It depends on who manufactures your BGA devices, where they get their solder
balls from and most importantly how good is your solder stenciling process....
From what I have seen in my facility, your +/- 0.001" is actually excellent
assuming that your tolerancing is derived statistically and not from standard
deviation data....
Marcelo
-----Original Message-----
From: Eric Christison [SMTP:[log in to unmask]]
Sent: Tuesday, October 13, 1998 10:55 AM
To: [log in to unmask]
Subject: [TN] Tolerance on Collapsed height of BGA Balls
I am having difficulty in believing something a packaging engineer is
telling me.
We have a design of sensor which is now BGA packaged. The balls are
0.030" diameter and 0.023" high.
After reflow I am assured that the collapsed height will be 0.019"
+/-0.001"(given a correctly
dimensioned footprint) . I have no problem with the 0.019", it's the
+/-0.001" that stretches my
credibility threshold.
Is there anyone out there that can confirm or deny this tolerance?
Regards,
Eric Christison
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|