Crepeau, Phil wrote:
>
> hi,
>
> there are several around. what you don't want to do is use an rtv
> adhesive/sealant that contains acetic anhydride/acetic acid.
>
> this is by no means an endorsement, but dow corning 3145 is a candidate. on
> the other hand, dow corning 732 is not one you'd want to use.
>
> phil crepeau
>
> -----Original Message-----
> From: Ken Patel [mailto:[log in to unmask]]
> Sent: Wednesday, October 14, 1998 11:42 AM
> To: [log in to unmask]
> Subject: [TN] RTV
>
> Can anyone recommend manufacturer and type of RTV to hold down components
> for communication application?
>
> re,
> Ken Patel
> ______________________________________________________
> Ken Patel Phone: (408) 490-6804
> 1708 McCarthy Blvd. Fax: (408) 490-6859
> Milpitas, CA 95035 Beeper: (888) 769-1808
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
> text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
> for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
Phil: Please explain your concern about RTV adhesives/sealants that
contain acetic anhydride/acetic acid. Dave F
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|