Crepeau, Phil wrote: > > hi, > > there are several around. what you don't want to do is use an rtv > adhesive/sealant that contains acetic anhydride/acetic acid. > > this is by no means an endorsement, but dow corning 3145 is a candidate. on > the other hand, dow corning 732 is not one you'd want to use. > > phil crepeau > > -----Original Message----- > From: Ken Patel [mailto:[log in to unmask]] > Sent: Wednesday, October 14, 1998 11:42 AM > To: [log in to unmask] > Subject: [TN] RTV > > Can anyone recommend manufacturer and type of RTV to hold down components > for communication application? > > re, > Ken Patel > ______________________________________________________ > Ken Patel Phone: (408) 490-6804 > 1708 McCarthy Blvd. Fax: (408) 490-6859 > Milpitas, CA 95035 Beeper: (888) 769-1808 > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following > text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section > for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or > 847-509-9700 ext.312 > ################################################################ > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. > For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 > ################################################################ Phil: Please explain your concern about RTV adhesives/sealants that contain acetic anhydride/acetic acid. Dave F ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################