Charles,
I do not believe there to have been too many changes.
The only materials I am aware of are:
Clay based which clog your filters and
Salt based which kill your cation/anion resins in minutes.
The only route is to direct your pre-wash to drain and re-circulate the wash
and rinse sections.
Unless someone else knows different............
Regards, Graham Naisbitt
[log in to unmask]
Concoat Ltd Phone: +44 1276 691100
Alasan House Fax: +44 1276 691227
Albany Park
CAMBERLEY
GU15 2PL UK
Any opinions expressed are those of this employer.
-----Original Message-----
From: Karalekas, Charles <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: 11 September 1998 15:32
Subject: [TN] Water soluble temporary solder mask
>I am seeking information on the feasibility of water soluble temporary
>solder mask in our process. We are using a closed loop water treatment
>system which, from all the information I have been able to gather, dooms it
>to failure due to the clay and other particulate matter in the masks which
>would clog our mixed bed treatment filters. Some of the other postings on
>Tech Net regarding this issue are a bit old and I was curious to see if
>there were any recent developments in the industry. A separate cleaning
>cycle would do the trick but its cost would not be justifiable versus
manual
>removal.
>Charles Karalekas
>Charles Karalekas
>Engineer Specialist
>Advanced Manufacturing Eng.
>& Material Evaluation
>Process Development
>Northrop Grumman
>847-259-9600 X6759
>FAX 847-506-7905
>E-Mail:[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|